Paint Defects——ALLIGATORING

2024-12-20 08:42

Paint Defects

一、ALLIGATORING)

1.Description:

Very large checking or cracking which resembles the skin of an alligator or crocodile. Cracks may penetrate through to the undercoat down to the substrate.
2.Probable Causes:

Internal stresses in the coating where the surface shrinks faster than the body of the paint film. Can be caused by excessive film thickness and limited paint flexibility. Also found on paint films having a soft undercoat with a hard topcoat.
3.Prevention:

Use correct coating specification and materials. Avoid excessive thickness. Avoid application at high ambient temperatures.
4.Repair:

Repair will depend upon size and extent of alligatoring. Abrade or remove all affected coats and apply suitable undercoat and topcoat. Follow recommended application procedures.





Disclaimer:The Institute of Plastic Research makes every effort to ensure the accuracy of the information, reliability of the data, and objectivity and fairness of the content and viewpoints described herein. However, we do not guarantee the accuracy and completeness of the information. Any losses or legal consequences resulting from actions taken based on this information are the sole responsibility of the individual undertaking them.